Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BNZ Materials BNZ-26-60 Insulating Firebrick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer BNZ Materials, Inc.
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BNZ Materials BNZ-26-60 Insulating Firebrick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirements and after firing is machined to precise tolerances. Made from high purity refractory clays and other ceramic raw materials, these IFB contain a carefully graded organic filler which is burned out during manufacture to give a uniform controlled pore structure.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Density 0.801 g/cc
0.0289 lb/in³
ASTM C134
Deformation 0.10 %
<br>@Temperature 1204 °C,<br> Time 5400 sec
0.10 %
<br>@Temperature 2199 °F,<br> Time 1.50 hour
10 psi load, Hot Load Strength; ASTM C16
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00130 GPa
0.189 ksi
ASTM C133
Compressive Strength 2.00 MPa
290 psi
Cold Crush Strength; ASTM C133
Thermal Properties Metric English Comments
CTE, linear 5.60 µm/m-°C
<br>@Temperature 20.0 - 1093 °C
3.11 µin/in-°F
<br>@Temperature 68.0 - 1999 °F
Thermal Conductivity 0.260 W/m-K
<br>@Temperature 260 °C
1.80 BTU-in/hr-ft²-°F
<br>@Temperature 500 °F
ASTM C182
0.290 W/m-K
<br>@Temperature 538 °C
2.01 BTU-in/hr-ft²-°F
<br>@Temperature 1000 °F
ASTM C182
0.300 W/m-K
<br>@Temperature 816 °C
2.08 BTU-in/hr-ft²-°F
<br>@Temperature 1500 °F
ASTM C182
0.330 W/m-K
<br>@Temperature 1093 °C
2.29 BTU-in/hr-ft²-°F
<br>@Temperature 1999 °F
ASTM C182
Maximum Service Temperature, Air 1427 °C
2601 °F
Normal oxidizing atmosphere
Shrinkage 0.20 %
<br>@Temperature 1399 °C,<br> Time 86400 sec
0.20 %
<br>@Temperature 2550 °F,<br> Time 24.0 hour
Permanent Linear Change; ASTM C210
Component Elements Properties Metric English Comments
Al2O3 60.4 %
60.4 %
CaO 0.10 %
0.10 %
Fe2O3 0.40 %
0.40 %
MgO 0.20 %
0.20 %
Na2O 1.8 %
1.8 %
Includes K&lt;sub&gt;2&lt;/sub&gt;O
SiO2 36.1 %
36.1 %
TiO2 1.0 %
1.0 %
Copyright © lookpolymers.com All Rights Reserved