Thermal Properties Metric English Comments
Vicat Softening Point 107 °C

@Load 5.001 kg
225 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYsan FL100 F20 SAN, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 107 °C

@Load 1.02 kg
225 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terluran® EGP-7 ABS
Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution
Vicat Softening Point 107 °C

@Load 0.999 kg
225 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled
ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 107 °C

@Load 5.00 kg
225 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim..
Vicat Softening Point 107 °C

@Load 1.00 kg
225 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibilac® PW-957 ASA Polymer
Injection
Vicat Softening Point 107 °C

@Load 1.00 kg
225 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Vicat Softening Point 107 °C

@Load 5.00 kg
225 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PG-383 Polystyrene
High heat; high strength
Vicat Softening Point 107 °C

@Load 5.00 kg
225 °F

@Load 11.0 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1616 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, good dimensional stabil..
Vicat Softening Point 107 °C

@Load 0.999 kg
225 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile
SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 107 °C

@Load 5.00 kg
225 °F

@Load 11.0 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact
Vicat Softening Point 107 °C

@Load 1.00 kg
225 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polyrex® PH-888H Polystyrene - High Impact