Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 316 °C | 600 °F | optimum use range |
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Intermittent |
Dielectric Polymers NT-590-2 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Mid-Mountain Materials HYTEX® 400 Kevlar® Industrial Textile Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy Silvaloy 45 is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A30 Brazing Alloy Silvaloy A30 does not contain cadmium and is often used as an alternate to cadmium containing alloys when the brazed assembly comes in contact with food or dairy products. Its slightly higher melt t.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A45 Brazing Alloy Silvaloy A45 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in the electrical industry and for brazing .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A45 Flux Coated Rod Brazing Alloy Silvaloy A45 FC is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is also used for brazing in electrical industry and for brazing b.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy Silvaloy A56T has the lowest brazing temperature, best wetting, and best flow of all the cadmium free alloys. It has a slight plastic range which may be noticed during melting on some applications. .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Greene Tweed CHEMRAZ® 551 Perfluoroelastomer With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz .. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvacap 35490 Brazing Alloy Silvacap is a low brazing temperature, cadmium-free alloy. It has a slight plastic range which may be noticed during melting on some applications. Generally, the joint strength using Silvacap will s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | intermittent |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Saint-Gobain Rulon® 125 Bearing/Seal PTFE Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Short Term |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | |
Master Bond Mastersil 801 One Component, Room Temperature Curing, Silicone System MasterSil 801 is an easy to use, one component, high performance silicone elastomer compound. MasterSil 801 features non-corrosive cure and serviceability up to 300°C; it exhibits good stability at.. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Maximum Service Temperature, Air | 316 °C | 600 °F | Continuous |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Maximum Service Temperature, Air | >= 316 °C | >= 600 °F | UL-746 B |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |