Saint-Gobain Meldin® 2001 Bearing

Category Polymer , Thermoset , Polyimide, TS
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 2001 Bearing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series can be machined into various confiations, from rod or sheet stock shapes. Black in color. Meldin 2000 Series offers very high compression strength, high creep resistance, and dimensional stability.Specific Notes on Meldin 2001 BearingMeldin 2001 is best suited for thermal and electrical insulation and radiation resistance. Meldin 2001 has the highest compressive strength properties of any material in the series.Applications include: Appliances, Automotive, Industrial, Semiconductor, Transportation.Specification Notes: Note that the specifications given for this product are typical specifications for the Meldin 2000 Series, and individual products will vary as indicated in the material notes.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Water Absorption 0.13 %
0.13 %
ASTM D570
Deformation 0.10 %

@Pressure 13.8 MPa
0.10 %

@Pressure 2000 psi
24 hrs. Mold Direction; ASTM D621
Outgassing - Total Mass Loss 0.010 %
0.010 %
% CVCM; ASTM E55955
1.04 %
1.04 %
% WVR; ASTM E595
1.62 %
1.62 %
% TML; ASTM E5955
Mechanical Properties Metric English Comments
Hardness, Shore D 92
92
ASTM D2240
Tensile Strength, Ultimate 20.6 MPa

@Temperature 316 °C
2990 psi

@Temperature 601 °F
ASTM D 638
48.2 MPa

@Temperature 260 °C
6990 psi

@Temperature 500 °F
ASTM D 638
92.0 MPa

@Temperature 23.0 °C
13300 psi

@Temperature 73.4 °F
ASTM D 638
Elongation at Break 7.0 %

@Temperature 260 °C
7.0 %

@Temperature 500 °F
ASTM D 638
8.0 %

@Temperature 23.0 °C
8.0 %

@Temperature 73.4 °F
ASTM D 638
25 %

@Temperature 316 °C
25 %

@Temperature 601 °F
ASTM D 638
Tensile Modulus 0.200 GPa

@Temperature 316 °C
29.0 ksi

@Temperature 601 °F
ASTM D 638
0.800 GPa

@Temperature 260 °C
116 ksi

@Temperature 500 °F
ASTM D 638
1.20 GPa

@Temperature 23.0 °C
174 ksi

@Temperature 73.4 °F
ASTM D 638
Flexural Strength 145 MPa
21000 psi
ASTM D 790
Flexural Modulus 4.40 GPa
638 ksi
ASTM D 790
Compressive Yield Strength 48.2 MPa

@Strain 7.00 %,
Temperature 316 °C
6990 psi

@Strain 7.00 %,
Temperature 601 °F
ASTM D695 Modified
75.8 MPa

@Strain 7.00 %,
Temperature 260 °C
11000 psi

@Strain 7.00 %,
Temperature 500 °F
ASTM D695 Modified
234 MPa

@Strain 10.0 %,
Temperature 23.0 °C
33900 psi

@Strain 10.0 %,
Temperature 73.4 °F
ASTM D695 Modified
Ultimate Compressive Strength 172.3 MPa

@Temperature 316 °C
24990 psi

@Temperature 601 °F
ASTM D695 Modified
203.3 MPa

@Temperature 260 °C
29490 psi

@Temperature 500 °F
ASTM D695 Modified
275.7 MPa

@Temperature 23.0 °C
39990 psi

@Temperature 73.4 °F
ASTM D695 Modified
Compressive Modulus 0.600 GPa

@Temperature 316 °C
87.0 ksi

@Temperature 601 °F
ASTM D695 Modified
1.20 GPa

@Temperature 260 °C
174 ksi

@Temperature 500 °F
ASTM D695 Modified
2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
ASTM D695 Modified
Izod Impact, Notched 0.283 J/cm
0.530 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C
29.4 µin/in-°F
ASTM E831-93
Thermal Conductivity 0.430 W/m-K
2.98 BTU-in/hr-ft²-°F
C518/C177
Maximum Service Temperature, Air >= 316 °C
>= 600 °F
UL-746 B
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 3.35

@Frequency 1.00e+6 Hz
3.35

@Frequency 1.00e+6 Hz
ASTM D150
3.39

@Frequency 10000 Hz
3.39

@Frequency 10000 Hz
ASTM D150
3.4

@Frequency 100 Hz
3.4

@Frequency 100 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm
400 kV/in
ASTM D149
Dissipation Factor 0.0016

@Frequency 100 Hz
0.0016

@Frequency 100 Hz
ASTM D150
0.0030

@Frequency 10000 Hz
0.0030

@Frequency 10000 Hz
ASTM D150
0.0039

@Frequency 1.00e+6 Hz
0.0039

@Frequency 1.00e+6 Hz
ASTM D150