Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Precision Polymer Engineering Z70M Hydrogenated NBR Compound Brown Hydrogenated Nitrile Rubber, 65-75 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1, where Z1 = Brown.Appl.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Precision Polymer Engineering Z85L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 81-90 °IRHD. Low acrylonitrile content.Applications: Specially compounded for service in low-temperature applications. High strength and excellent chem.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 350 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Intermittent |
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Silikony Polskie Gumosil E Silicone Rubber Very flexible with low hardness |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2514S-20-10 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2518S-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2526S-30-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi.. |
|||
Maximum Service Temperature, Air | >= 180 °C | >= 356 °F | Exotherm Temp; Method 4 |
Lubrizol Telene 1610 A/B & A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | Short peaks operation |
Polyram PlusTek PB150 Nylon 6, Injection Molding Fast cycle polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | <= 180 °C | <= 356 °F | a few hours operation |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) at 50% RH Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Dow Corning 738 ELECTRICAL SEALANT. WHITE Durable general purpose sealant/adhesive for a wide variety of bonding and sealing applications. Can be used in applications where mil spec is required.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | short term; EMS |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
BASF Ultramid® B3K BK00464 PA6 (Dry) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
Rogers Corporation Bisco® A2 R 1.5 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |
|||
Maximum Service Temperature, Air | 180 - 200 °C | 356 - 392 °F | Average value: 190 °C Grade Count:4 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Maximum Service Temperature, Air | 180 °C | 356 °F | <20000 hours; IEC 60216-P1 |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Maximum Service Temperature, Air | 180 - 300 °C | 356 - 572 °F | |
SMAC CABLE® 2524S-40-08 Damping Material The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro.. |