Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Nylacast Moly Cast Nylon 6, MoS2 Filled Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Nanosonic Metal Rubber™ Metal Rubber™ is a unique self-assembled nanocomposite material that combines the high electrical conductivity of metals with the low mechanical modulus of elastomers. Self-assembly processing allo.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | < 50 h; IEC 60216/T1 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Short Time; IEC 60216 |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Short Time; IEC 60216 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Short Time; IEC 60216 |
PolyOne Bergadur™ PB40 G20 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short period, no load |
Omnia Plastica PA6 GF Akulon GF - Dry Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | 20,000 h; IEC 216/T1 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | <20000 hours; IEC 60216-P1 |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Maximum Operating Temperature |
Industrial Laminates/Norplex NP185 Carbon Fiber
(discontinued **) Description: NP185, aramid fiber fabric/phenolic surfaces (2 ply each side) on NP504 core material. Excellent mechanical properties at elevated temperatures and in adverse environments. Used as wear.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | <20000 hours; IEC 60216-P1 |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Maximum Service Temperature, Air | 170 °C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
338 °F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
Teknor Apex Sinvicomp SFE 4500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Continuous Use |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Chesterton 622 White Grease Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Atom Adhesives AA-DUCT 903 Epoxy Adhesive AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | <20000 hours; IEC 60216-P1 |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |