Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 220 °C | 428 °F | Continuous |
Pyrotek TS-235 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | < 50 h; IEC 216/T1 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Short Time; IEC 60216 |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Short Time; IEC 60216 |
PolyOne Bergamid™ A70 GK30 H Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Greene Tweed CHEMRAZ® 514 Perfluoroelastomer Greene Tweed’s Chemraz® 514, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 514 offers a Shor.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance an.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Pigment Heat Resistance; EN 12877-3 |
Karina 18/268-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Maximum Service Temperature, Air | 220 - 240 °C | 428 - 464 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | 220°C insulation by UL, the US Navy, and other tests |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | 220°C insulation by UL, the US Navy, and other tests |
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | 220°C insulation by UL, the US Navy, and other tests |
DuPont™ Nomex® 410 Paper, 25.5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Electrical insulation |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Electrical insulation |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | Electrical insulation |
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short term; EMS |
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60 Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | short cycle operations |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Maximum Service Temperature, Air | 220 °C | 428 °F | |
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |