Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | no load |
McDanel Advanced Ceramics 99.8% Alumina Information provided by McDanel Advanced Ceramic Technologies |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast AC 85-5 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast AK 98 Dense Refractory Brick Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Momentive Performance Materials HTR1002 PBN/PG Heating Element PBN/PG resistance heating elements combine the unique electrical, chemical, and thermal properties of PBN, a dielectric material, and Pyrolytic Graphite (PG), an electrical conductor, to produce a t.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Momentive Performance Materials HTR1003 PBN/PG Heating Element PBN/PG resistance heating elements combine the unique electrical, chemical, and thermal properties of PBN, a dielectric material, and Pyrolytic Graphite (PG), an electrical conductor, to produce a t.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Momentive Performance Materials HTR1004 PBN/PG Heating Element PBN/PG resistance heating elements combine the unique electrical, chemical, and thermal properties of PBN, a dielectric material, and Pyrolytic Graphite (PG), an electrical conductor, to produce a t.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sinotek Materials HFB Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | Continuous |
Unifrax Fibermax® Duraboard® 18H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | Continuous |
Unifrax Fibermax® Duraboard® 18R Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Du-Co Ceramics S-699 Alumina Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories LPCT-18PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories MMCT-95 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-90SC High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | limited |
Chosun Refractories SFC-90W High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide This grade offers a high flexural strength for a zirconia. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear re.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide Full-fired, fine grain, high purity MgO ceramic. Inert to molten metals, slags, superconductors. Broad line of standard crucibles. Custom parts made to print. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95% This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for se.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |
|||
Maximum Service Temperature, Air | 1800 °C | 3270 °F | |
Anderman Ceramics EZY 88 Zirconia, 88%, Fully Yttria-Stabilized Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |