Unifrax Fibermax® Duraboard® 18R Board

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Unifrax I LLC
Trade Name Fibermax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fibermax® Duraboard® 18R Board.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. Another benefit of these board products is their extremely high modulus of rupture (MOR) in both the green and fired state. Because of their strength, both Duraboard 1700 and Duraboard 1800 are very well suited for applications where sag resistance is critical. Duraboard 17R and 18R have a rolled finish, while Duraboard 17H and 18H are compressed during manufacturing for optimum density and sanded smooth. Standard thicknesses available for these products are 13mm, 25mm, 38mm, and 50mm.Typical ApplicationsHigh-temperature laboratory furnaces/kilnsDiffusion FurnacesKiln setter tilesSpecialty shapesAtmosphere furnacesElectric furnacesInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.513 g/cc
0.0185 lb/in³
Dry
Loss On Ignition 4.0 %

@Temperature 1260 °C,
Time 86400 sec
4.0 %

@Temperature 2300 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00137 GPa
0.198 ksi
Fired
0.00176 GPa
0.255 ksi
Green
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1800 °C
3270 °F
Continuous
Shrinkage 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
Linear
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
SiO2 15 %
15 %
Descriptive Properties Value Comments
Appearance White