Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | <= 1400 °C | <= 2550 °F | |
Plansee TZM Titanium-Zirconium-Molybdenum Molybdenum is alloyed with Titanium and Zirconium and is doped with extremely fine carbides to create TZM.Characteristics:Higher strength than pure MoHigher recrystallization temperature than pure M.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
GBC Grade 90 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics 0.5 Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics REFCAST Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics THERMO PATCH Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Specialty Materials SCS-6 Silicon Carbide Monofilament High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced tit.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sapco Silicon Nitride, Si3N4 Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Sharadaa Ceramics HICCS Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
CoorsTek Porcelain Information provided by CoorsTek. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories CT-140 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%) Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".Information provided by Anderman Cerami.. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
Anderman Ceramics EM60P Sillimanite Porous synthetic mullite with high thermal shock. Available as tube up to 10 ft (3 m) long with diameters 0.6" to 2.4".Information provided by Anderman Ceramics. |
|||
Maximum Service Temperature, Air | 1400 °C | 2550 °F | |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |