| Category | Ceramic |
| Manufacturer | CoorsTek |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | CoorsTek Porcelain.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.40 g/cc | 0.0867 lb/in³ | ASTM C20 |
| Water Absorption | 0.00 % | 0.00 % | ASTM C373 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Knoop Microhardness | 5.9 | 5.9 | 1000 g load |
| Hardness, Rockwell 45 N | 60 | 60 | GPa |
| Modulus of Elasticity | 104 GPa | 15100 ksi | ASTM C848 |
| Flexural Strength | 130 MPa | 18900 psi | ASTM F417 |
| Compressive Strength | 590 MPa | 85600 psi | ASTM C773 |
| Fracture Toughness | 2.00 MPa-m½ | 1.82 ksi-in½ |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 9.50 µm/m-°C <br>@Temperature 25.0 - 1000 °C |
5.28 µin/in-°F <br>@Temperature 77.0 - 1830 °F |
ASTM C372 |
| Thermal Conductivity | 5.00 W/m-K | 34.7 BTU-in/hr-ft²-°F | ASTM C408 |
| Maximum Service Temperature, Air | 1400 °C | 2550 °F | No Load |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 5.9 <br>@Frequency 1e+6 Hz |
5.9 <br>@Frequency 1e+6 Hz |
|
| Dielectric Loss Index | 0.0024 | 0.0024 | at 25°C, 1 MHz; ASTM D2520 |