Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | RT |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | RT |
Outokumpu 4438 High Performance Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | RT |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | ASTM D 5470 |
Fujipoly Industries Sarcon® XR-j Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 - 100 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 - 100 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | in plane; ASTM E1461 |
DSM Stanyl® TC551 PA46 FR(17) Thermal conductive material, Flame Retardant |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/35 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | |
Cytec Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Thermal Conductivity | 14.0 - 20.0 W/m-K | 97.2 - 139 BTU-in/hr-ft²-°F | |
Blasch Ceramics NITRON Nitride bonded SiC Features:Properties suit many severe operating conditionsGood wear and abrasionResists wetting by non-ferrous metalsHigh mechanical strengthExcellent Thermal shock resistance |
|||
Thermal Conductivity | >= 14.0 W/m-K | >= 97.2 BTU-in/hr-ft²-°F | |
Advanced Ceramics ALC 1081 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 398J Yttrium Oxide Ceralloy® 398J Hot Pressed Yttrium Oxide is a high purity hot-pressed ceramic exhibiting excellent corrosion and erosion resistance. Products produced from Hot Pressed Yttrium Oxide are for semicon.. |
|||
Thermal Conductivity | 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | in plane; ASTM E1461 |
DSM Stanyl® TC502 PA46 Thermal conductive material |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel UREA 25.22.2 Plants Description: CLI UREA 25.22.2 chemical composition has been optimized for specific uses in Urea plants. It is a 310L modified austenitic stainless steel with low carbon, low silicon and high nitroge.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 20.0 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |