Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling)

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , Precipitation Hardening Stainless , T S10000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name VIRGO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosion resistance. The VIRGO 15.5 PH grade is similar to the VIRGO 17.4 PH grade having equivalent mechanical properties. Due to the lower Chromium content and increased Nickel content the VIRGO 15.5 PH grade contains less ferrite which provides better through thickness properties particularly when considering thick plates. The corrosion behavior is close to 304 grade and better than 410 grade. The main applications are those of VIRGO 17.4 PH grade i.e. mechanical components and offshore industry when considering heavy plates.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 197 GPa
28600 ksi
Tensile Modulus 77.0 GPa
11200 ksi
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 0.000 - 100 °C
6.00 µin/in-°F

@Temperature 32.0 - 212 °F
11.0 µm/m-°C

@Temperature 0.000 - 100 °C
6.11 µin/in-°F

@Temperature 32.0 - 212 °F
11.6 µm/m-°C

@Temperature 0.000 - 400 °C
6.44 µin/in-°F

@Temperature 32.0 - 752 °F
12.0 µm/m-°C

@Temperature 0.000 - 500 °C
6.67 µin/in-°F

@Temperature 32.0 - 932 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 14.0 W/m-K

@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 15 %
15 %
Copper, Cu 3.5 %
3.5 %
Iron, Fe 76.63 - 76.7 %
76.63 - 76.7 %
As remainder
Nickel, Ni 4.5 %
4.5 %
Niobium, Nb (Columbium, Cb) 0.30 %
0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F
Users viewing this material also viewed the following: