Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name CLC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains some residual ferrite (= 2%) after solution annealing (1100 - 1150°C / 2012 - 2102°F) and water quenching. Its low carbon content avoids the intergranular corrosion, even on welded pieces without an ulterior water quenching. The high Molybdenum content gives this steel a higher resistance to corrosion in chlorides environments than standard grades (CLC17-12-2L / 316L). Nitrogen additions improves structure stability, increases the yield strength and improves pitting and crevice corrosion resistance when compared to CLC 18-15-4L (317L). Its main properties are : high ductility and improved corrosion resistance. The main applications are chemical and petrochemical applications, pollution control equipments and chemical tankers.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 590 MPa
>= 85600 psi
Tensile Strength, Yield >= 290 MPa

@Strain 0.200 %
>= 42100 psi

@Strain 0.200 %
>= 315 MPa

@Strain 1.00 %
>= 45700 psi

@Strain 1.00 %
Elongation at Break >= 40 %
>= 40 %
Modulus of Elasticity 200 GPa

@Temperature 20.0 - 100 °C
29000 ksi

@Temperature 68.0 - 212 °F
Poissons Ratio 0.299
0.299
Calculated
Shear Modulus 77.0 GPa

@Temperature 20.0 - 100 °C
11200 ksi

@Temperature 68.0 - 212 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.89 µin/in-°F

@Temperature 68.0 - 212 °F
16.5 µm/m-°C

@Temperature 20.0 - 200 °C
9.17 µin/in-°F

@Temperature 68.0 - 392 °F
17.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 µin/in-°F

@Temperature 68.0 - 572 °F
18.0 µm/m-°C

@Temperature 20.0 - 500 °C
10.0 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C

@Temperature 20.0 - 100 °C
0.120 BTU/lb-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 14.0 W/m-K

@Temperature 20.0 - 100 °C
97.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 18.2 %
18.2 %
Iron, Fe 65.43 - 65.46 %
65.43 - 65.46 %
As remainder
Molybdenum, Mo 3.2 %
3.2 %
Nickel, Ni 13 %
13 %
Nitrogen, N 0.14 %
0.14 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 - 100 °C
0.0000800 ohm-cm

@Temperature 68.0 - 212 °F