| Category | Polymer , Thermoplastic , Nylon , Nylon 46 |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Stanyl® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Stanyl® TC502 PA46.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 2.00 % | 2.00 % | Sim. To ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 65.0 MPa | 9430 psi | dry; ISO 527-1/-2 |
| Elongation at Break | 1.1 % | 1.1 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 9.00 GPa | 1310 ksi | dry; ISO 527-1/-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.0 µm/m-°C | 13.9 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | dry; ISO 11359-1/-2 |
| Thermal Conductivity | 2.10 W/m-K | 14.6 BTU-in/hr-ft²-°F | through plane; ASTM E1461 |
| 14.0 W/m-K | 97.2 BTU-in/hr-ft²-°F | in plane; ASTM E1461 | |
| Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+6 ohm-cm | 1.00e+6 ohm-cm | dry; IEC 60093 |