Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compounding |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | HOT-DISK || 60x60x3 mm |
Lehmann & Voss LUVOCOM® 1/CF/40 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | Longitudinal |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is fr.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.70 BTU-in/hr-ft²-°F | |
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; ASTM E 1530 |
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | Silicone Property; ASTM E1530 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
silicone property; ASTM E1530 |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-022 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-022 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Thermal Conductivity | 1.40 W/m-K @Temperature 100 °C |
9.72 BTU-in/hr-ft²-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-022 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |
|||
Thermal Conductivity | 1.40 W/m-K | 9.72 BTU-in/hr-ft²-°F | silicone property; ASTM E1530 |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |