Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV88 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon POM C Polyacetal C Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | ASTM C177 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612-1 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |