| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | Isoflon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Isoflon POM C Polyacetal C.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | DIN 53479 |
| Water Absorption | 0.22 % | 0.22 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength | 65.0 MPa | 9430 psi | DIN 53455 |
| Elongation at Break | 25 % | 25 % | DIN 53455 |
| Tensile Modulus | 2.90 GPa | 421 ksi | DIN 53457 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | DIN 52328 |
| Thermal Conductivity | 0.310 W/m-K | 2.15 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 165 °C | 329 °F | DIN 53736 |
| Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous; DIN 52612 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | |
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous; DIN 52612 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | DIN 53482 |
| Dielectric Constant | 3.7 @Frequency 1000 Hz |
3.7 @Frequency 1000 Hz |
DIN 53483 |
| Dielectric Strength | 20.0 - 65.0 kV/mm | 508 - 1650 kV/in | DIN 53481 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Nat./Black |