Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM E831 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM E831 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® S 131 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE) Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Borealis RA130E-2491 Polypropylene Random Copolymer RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber 30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber 30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | Moulding Direction; ASTM C177 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl .. |
|||
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element.. |