| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled |
| Manufacturer | Polyram |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | DIN 53479 |
| Water Absorption | 0.070 % | 0.070 % | DIN 53495 |
| Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | |
| Melt Flow | 3.5 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
3.5 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 110 MPa | 16000 psi | ASTM-D638 |
| Elongation at Break | 2.0 % | 2.0 % | ASTM-D638 |
| Flexural Strength | 195 MPa | 28300 psi | ASTM D790 |
| Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM-D790 |
| Izod Impact, Notched | 1.30 J/cm <br>@Temperature 23.0 °C |
2.44 ft-lb/in <br>@Temperature 73.4 °F |
ASTM-D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
| Deflection Temperature at 0.46 MPa (66 psi) | 147 °C | 297 °F | DIN 53461 |
| Deflection Temperature at 1.8 MPa (264 psi) | 139 °C | 282 °F | DIN 53461 |
| Flammability, UL94 | V-1 <br>@Thickness 3.00 mm |
V-1 <br>@Thickness 0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | DIN 53482 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | DIN 53482 |
| Dielectric Constant | 3.3 <br>@Frequency 1e+6 Hz |
3.3 <br>@Frequency 1e+6 Hz |
VDE 0303/4 |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | VDE 0303/4 |