Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.17 g/cc
0.0784 lb/in³
ASTM D792
Apparent Bulk Density 0.880 g/cc
0.0318 lb/in³
ASTM D4894
Water Absorption 0.00 %
0.00 %
ASTM D570
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.0 MPa
4790 psi
ASTM D638
Elongation at Break 310 %
310 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Flammability, UL94 V-0
V-0
VE-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 60.0 - 2.00e+9 Hz
2.1

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150
Dielectric Strength 60.0 kV/mm
1520 kV/in
ASTM D149
Dissipation Factor >= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
>= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150