Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Wolf Kunststoff
Trade Name ZEDEX®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zedex
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ISO 1183
Water Absorption 0.020 %
<br>@Temperature 23.0 °C
0.020 %
<br>@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.040 %
0.040 %
DIN EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore A >= 100
>= 100
DIN 53505
Hardness, Shore D 60
60
DIN 53505
Ball Indentation Hardness 32.0 MPa
4640 psi
DIN 2039
Tensile Strength at Break 12.0 MPa
1740 psi
DIN EN ISO 527
Tensile Strength 12.0 MPa
1740 psi
DIN EN ISO 527
Tensile Stress 0.600 MPa
<br>@Strain 1.00 %,<br> Time 3.60e+6 sec
87.0 psi
<br>@Strain 1.00 %,<br> Time 1000 hour
DIN 53444
Tensile Strength, Yield 6.80 MPa
986 psi
Elastic Limit
Elongation at Break 192 %
192 %
192 %
192 %
DIN EN ISO 527
Elongation at Yield 3.3 %
3.3 %
Flexural; DIN EN ISO 178
4.2 %
4.2 %
Elastic Yield Point
Tensile Modulus 0.850 GPa
123 ksi
DIN EN ISO 527
Flexural Strength 15.0 MPa
2180 psi
Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
15.0 MPa
2180 psi
DIN EN ISO 178
Flexural Modulus 1.19 GPa
173 ksi
DIN EN ISO 178
Compressive Strength 11.0 MPa
1600 psi
Elastic Limit
0.800 MPa
<br>@Time 3.60e+7 sec
116 psi
<br>@Time 10000 hour
8.00 MPa
<br>@Time 360000 sec
1160 psi
<br>@Time 100 hour
10.0 MPa
<br>@Time 36.0 sec
1450 psi
<br>@Time 0.0100 hour
19.0 MPa
<br>@Strain 3.50 %
2760 psi
<br>@Strain 3.50 %
DIN EN ISO 604
Compressive Modulus 1.15 GPa
167 ksi
DIN EN ISO 604
Fatigue Strength 4.00 MPa
<br>@# of Cycles 1.00e+6
580 psi
<br>@# of Cycles 1.00e+6
1 Hz
K Factor (ISO) 0.60 µm/km
<br>@Temperature 20.0 °C
0.60 µm/km
<br>@Temperature 68.0 °F
0.80 µm/km
<br>@Temperature 200 °C
0.80 µm/km
<br>@Temperature 392 °F
2.7 µm/km
<br>@Temperature 100 °C
2.7 µm/km
<br>@Temperature 212 °F
6.4 µm/km
<br>@Temperature 240 °C
6.4 µm/km
<br>@Temperature 464 °F
Charpy Impact Unnotched NB
NB
EN ISO 179/1eU
Charpy Impact, Notched 11.3 J/cm²
53.8 ft-lb/in²
EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.10
<br>@Temperature 20.0 °C
0.10
<br>@Temperature 68.0 °F
Dry Operation
0.10
<br>@Temperature 100 °C
0.10
<br>@Temperature 212 °F
Dry Operation
Coefficient of Friction, Static 0.17
<br>@Temperature 20.0 °C
0.17
<br>@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 61.0 MPa
8850 psi
At 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.02783 MPa-m/sec
794.5 psi-ft/min
v = 1m/min
0.100 MPa-m/sec
2860 psi-ft/min
v = 200m/min
0.20833 MPa-m/sec
5947.8 psi-ft/min
v = 10m/min
0.43333 MPa-m/sec
12372 psi-ft/min
v = 100m/min
Compression Set 1.4 %
1.4 %
Elastic Compression Limit
Thermal Properties Metric English Comments
CTE, linear 144 µm/m-°C
<br>@Temperature <=100 °C
80.0 µin/in-°F
<br>@Temperature <=212 °F
ISO E 830
192 µm/m-°C
<br>@Temperature <=150 °C
107 µin/in-°F
<br>@Temperature <=302 °F
ISO E 831
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
DSC
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 323 °C
613 °F
DSC
Maximum Service Temperature, Air 70.0 °C
158 °F
Pressed Bushings
240 °C
464 °F
Continuous
260 °C
500 °F
Short Term (3h)
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
DSC
Flammability, UL94 V-0
V-0
Oxygen Index 75 %
75 %
DIN EN ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
IEC 93
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 93
Dielectric Constant 2.7
<br>@Frequency 110 Hz
2.7
<br>@Frequency 110 Hz
IEC 250
Dielectric Strength 21.0 kV/mm
533 kV/in
IEC 243
Dissipation Factor 0.00030
0.00030
IEC 112
0.175
<br>@Frequency 1.00 Hz
0.175
<br>@Frequency 1.00 Hz
Comparative Tracking Index 42 V
42 V
IEC 112
Descriptive Properties Value Comments
Alignment Adjustment 2
Nominal Scale: 1, low; 10, high
Chemical Sterilization 10
Nominal Scale: 1, low; 10, high
Color Green
Creep Resistance 1
Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion 1
Nominal Scale: 1, low; 10, high
Free from Silicon Applicable
High Precision Bushings (negative clearance) Applicable
Machined Parts Applicable
Moist Heat Sterilization 10
Nominal Scale: 1, low; 10, high
Resistance Against dust, Dirt, Abrasive Substances 2
Nominal Scale: 1, low; 10, high
Resistance Against Hot Water 150
Resistance to Chemicals 9
Nominal Scale: 1, low; 10, high
Resistant Against Disinfectant Applicable
Rods up to Øe (de) Applicable
Sheets up to Maximum Thickness Applicable
Sliding Velocity 150
Suitable for Outdoor Use 10
Nominal Scale: 1, low; 10, high
Suitable for Use in Water Applicable
Suitable for Vacuum Applicable
UV Rays Resistance 9
Nominal Scale: 1, low; 10, high
UV-Sterilization 7
Nominal Scale: 1, low; 10, high