Polymer Property : Thermal Conductivity = 0.180 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
DIN 52612
Polycasa XT PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
DIN 52612
Polycasa XT 610 PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East)
LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating.
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer  (discontinued **)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer  (Unverified Data**)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® CL101 PBT+PC
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East)
Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East)
XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I.
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XD1507S PBT+PC (Europe-Africa-Middle East)
XENOY XD1507S is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties, designed for self coloured, optiwall bumper facias.This data was supplie..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East)
XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East)
PBT+PC blend for painted automotive exterior applications, having good flow.
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East)
Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XL1339U PC+PET (Europe-Africa-Middle East)
XENOY XL1339U is an unreinforced amorphous PC+PET blend, offering excellent impact performance over a wide temperature range. It combines very good flow characteristics with high heat resistance. XL..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East)
XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Thermal Conductivity 0.180 W/m-K

@Temperature 650 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 1200 °F
ASTM C177
Unifrax IsoMat® AV/AVi Substrate Support Mat
Developed to meet the most stringent European regulatory requirements, IsoMat AV/Avi is engineered utilizing the unique Isofrax® 1260°C fibers - a revolutionary green fiber produced using patented..
Thermal Conductivity 0.180 W/m-K

@Temperature 650 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 1200 °F
ASTM C177
Unifrax IsoMat® AV5 Substrate Support Mat
IsoMat AV5 is designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.IsoMat AV5 offers superior performance at low tem..
Thermal Conductivity 0.180 W/m-K

@Temperature 650 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 1200 °F
ASTM C177
Unifrax XPE® AV2/AV2i Substrate Support Mat
XPE®-AV2 is an advanced intumescent expanding mat designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation. When compa..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
Westlake Plastics Imidex Thermoplastic Polyimide
Made from Aurum® resin. Applications include electronics, acoustics, composites, wire/cable insulation, adhesive film, and washers/gaskets. It will not melt unto itself, is thermoformable, has hi..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
Elisto THERMOSTAR® 4000 Mold Insulation Material
Insulation of clamping platesInformation provided by elisto
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
cured
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating
QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par..
Thermal Conductivity 0.180 W/m-K

@Temperature 45.0 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 113 °F
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Thermal Conductivity 0.180 W/m-K

@Temperature 45.0 °C
1.25 BTU-in/hr-ft²-°F

@Temperature 113 °F
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ASTM E1530
3M Scotchcast™ 265 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing ..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and ..
Thermal Conductivity 0.180 W/m-K
1.25 BTU-in/hr-ft²-°F
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..