NeXolve CORIN XLS Polyimide

Category Polymer , Film , Thermoset , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer NeXolve Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NeXolve CORIN XLS Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resistant to radiation and atomic oxygen erosion. NeXolve’s CORIN XLSPolyimide is a colorless, clear, organic/inorganic sprayable nanocomposite that is resistant to radiation and atomic oxygen erosion. CORIN XLS Polyimide is ideal for use in national security applications, such as satellites, and also in solar panels and light-emitting organic displays.CORIN XLS Polyimide combines polyimide and nanocomposite technologies to deliver unsurpassed levels of optical clarity and oxidative stability, as well as stability to solar radiation. This fluorinated polyimide nanocomposite offers the highest atomic oxygen (AO) durability as well as the highest light transmission of all the CORIN grades, making it an ideal lightweight substitute material for glass used in space polyvoltaic (PV) arrays in low earth orbit (LEO). CORIN XLS Polyimide exhibits a glass transition temperature in excess of 250°C and can be used as a replacement for glass substrates in display applications.CORIN XLS Polyimide can be processed with organic solvents for spray, dip or casting applications as well as with hot isostatic press (HIP). This multipurpose material is available in film (standard thicknesses of 0.5 mil and 1.0 mil, other thicknesses available), solvent-based liquid resin or powder form.CORIN XLS Polyimide is manufactured in continuous rolls of 0.1, 0.25, 0.50, and 1.0 mil thickness. CORIN XLS Polyimide is optically transparent and exhibits a glass transition temperature greater than 250 degrees centigrade.Information Provided by NeXolve Corporation.
Mechanical Properties Metric English Comments
Tensile Strength 74.0 MPa

@Thickness 0.0250 mm
10700 psi

@Thickness 0.000984 in
ASTM D882-02
Elongation at Break 8.0 %

@Thickness 0.0250 mm
8.0 %

@Thickness 0.000984 in
ASTM D882-02
Tensile Modulus 2.10 GPa

@Thickness 0.0250 mm
305 ksi

@Thickness 0.000984 in
ASTM D882-02
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Thickness 1.00 mm,
Temperature 125 - 175 °C
37.8 µin/in-°F

@Thickness 0.0394 in,
Temperature 257 - 347 °F
ASTM E831-06
Glass Transition Temp, Tg 251 °C
484 °F
DMA; ASTM E1356-03
266 °C
511 °F
DSC; ASTM E1356-03
Optical Properties Metric English Comments
Refractive Index 1.54

@Wavelength 589 nm
1.54

@Wavelength 589 nm
Abbe; ASTM D542-00
UV Transmittance 50 %

@Thickness 0.0120 mm,
Wavelength 377 nm
50 %

@Thickness 0.000472 in,
Wavelength 377 nm
50% Transmission UV Cutoff
50 %

@Thickness 0.0250 mm,
Wavelength 392 nm
50 %

@Thickness 0.000984 in,
Wavelength 392 nm
50% Transmission UV Cutoff
50 %

@Thickness 0.0380 mm,
Wavelength 407 nm
50 %

@Thickness 0.00150 in,
Wavelength 407 nm
50% Transmission UV Cutoff
Descriptive Properties Value Comments
Solar Absorptivity 0.08
1 mil thickness; ASTM E903-96