Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.0 µm/m-°C | 8.33 µin/in-°F | X-Direction; TMA; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 6202 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
CTE, linear | 15.0 µm/m-°C | 8.33 µin/in-°F | Y-Direction; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
CTE, linear | 15.0 - 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.33 - 11.1 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
CTE, linear | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
CTE, linear | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
CTE, linear | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
CTE, linear | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
CTE, linear | 15.0 - 15.0 µm/m-°C @Temperature 55.0 - 160 °C |
8.33 - 8.33 µin/in-°F @Temperature 131 - 320 °F |
Average value: 15.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 15.0 - 42.3 µm/m-°C | 8.33 - 23.5 µin/in-°F | Average value: 24.0 µm/m-°C Grade Count:31 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
CTE, linear | 15.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
CTE, linear | 15.0 µm/m-°C | 8.33 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1/XCF/20 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 - 100 °C |
8.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCOLOY® Alloy DS A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista.. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 140 °F |
|
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
CTE, linear | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-2 |
Unitika RUN35-C25 PA6, Dry High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
CTE, linear | 15.0 - 17.0 µm/m-°C @Temperature 1000 °C |
8.33 - 9.44 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-309NM,Insert Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel 220 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel 5900 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel Alloy 120 Nickel Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.0 - 20.0 µm/m-°C | 8.33 - 11.1 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm.. |
|||
CTE, linear | 15.0 - 25.0 µm/m-°C | 8.33 - 13.9 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
CTE, linear | 15.0 - 25.0 µm/m-°C | 8.33 - 13.9 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote.. |
|||
CTE, linear | 15.0 µm/m-°C | 8.33 µin/in-°F | y direction |
Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |
|||
CTE, linear | 15.0 - 25.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.33 - 13.9 µin/in-°F @Temperature 122 - 302 °F |
Average value: 19.2 µm/m-°C Grade Count:3 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 15.0 - 53.0 µm/m-°C @Temperature 40.0 - 130 °C |
8.33 - 29.4 µin/in-°F @Temperature 104 - 266 °F |
Average value: 29.6 µm/m-°C Grade Count:12 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 15.0 - 17.0 µm/m-°C | 8.33 - 9.44 µin/in-°F | IPC TM-650 2.4.41 |
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |