Overview of materials for Melamine-Phenolic Copolymer

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Melamine-Phenolic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.50 - 1.81 g/cc
0.0542 - 0.0654 lb/in³
Average value: 1.64 g/cc Grade Count:22
Apparent Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Average value: 0.655 g/cc Grade Count:11
Water Absorption 0.220 - 2.50 %
0.220 - 2.50 %
Average value: 1.18 % Grade Count:21
Linear Mold Shrinkage -0.000500 - 0.0130 cm/cm
-0.000500 - 0.0130 in/in
Average value: 0.00732 cm/cm Grade Count:22
Mechanical Properties Metric English Comments
Hardness, Rockwell E 67.0 - 86.0
67.0 - 86.0
Average value: 75.8 Grade Count:11
Tensile Strength, Ultimate 53.0 - 76.0 MPa
7690 - 11000 psi
Average value: 61.7 MPa Grade Count:12
Tensile Strength, Yield 40.0 - 90.0 MPa
5800 - 13100 psi
Average value: 61.0 MPa Grade Count:10
Elongation at Break 0.470 - 0.950 %
0.470 - 0.950 %
Average value: 0.745 % Grade Count:11
Modulus of Elasticity 5.00 - 13.3 GPa
725 - 1930 ksi
Average value: 8.90 GPa Grade Count:22
Flexural Yield Strength 70.0 - 140 MPa
10200 - 20300 psi
Average value: 101 MPa Grade Count:22
Flexural Modulus 5.00 - 12.5 GPa
725 - 1810 ksi
Average value: 8.93 GPa Grade Count:22
Compressive Yield Strength 142 - 250 MPa
20600 - 36300 psi
Average value: 194 MPa Grade Count:22
Izod Impact, Notched 0.159 - 0.215 J/cm
0.298 - 0.403 ft-lb/in
Average value: 0.186 J/cm Grade Count:11
Charpy Impact Unnotched 0.450 - 1.40 J/cm²
2.14 - 6.66 ft-lb/in²
Average value: 0.812 J/cm² Grade Count:11
0.400 - 0.700 J/cm²

@Temperature -40.0 - -40.0 °C
1.90 - 3.33 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 0.550 J/cm² Grade Count:1
Charpy Impact, Notched 0.120 - 0.239 J/cm²
0.571 - 1.14 ft-lb/in²
Average value: 0.181 J/cm² Grade Count:22
Thermal Properties Metric English Comments
CTE, linear 15.0 - 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
8.33 - 29.4 µin/in-°F

@Temperature 104 - 266 °F
Average value: 29.6 µm/m-°C Grade Count:12
Thermal Conductivity 0.400 - 0.600 W/m-K
2.78 - 4.16 BTU-in/hr-ft²-°F
Average value: 0.470 W/m-K Grade Count:10
0.510 - 0.610 W/m-K

@Temperature 100 - 100 °C
3.54 - 4.23 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.570 W/m-K Grade Count:4
Maximum Service Temperature, Air 135 - 190 °C
275 - 374 °F
Average value: 150 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 155 - 202 °C
311 - 396 °F
Average value: 178 °C Grade Count:21
Deflection Temperature at 8.0 MPa 110 - 140 °C
230 - 284 °F
Average value: 123 °C Grade Count:11
Flammability, UL94 V-0 - 5VB
V-0 - 5VB
Grade Count:21
Oxygen Index 33.0 - 36.0 %
33.0 - 36.0 %
Average value: 34.2 % Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+14 ohm-cm
1.00e+11 - 1.00e+14 ohm-cm
Average value: 1.63e+13 ohm-cm Grade Count:22
Surface Resistance 1.00e+10 - 1.00e+12 ohm
1.00e+10 - 1.00e+12 ohm
Average value: 1.04e+11 ohm Grade Count:11
Dielectric Constant 6.50 - 16.0
6.50 - 16.0
Average value: 9.33 Grade Count:22
Dielectric Strength 4.80 - 30.0 kV/mm
122 - 762 kV/in
Average value: 12.3 kV/mm Grade Count:21
Dissipation Factor 0.0300 - 0.500
0.0300 - 0.500
Average value: 0.160 Grade Count:22
Arc Resistance 115 - 188 sec
115 - 188 sec
Average value: 172 sec Grade Count:14
Comparative Tracking Index 175 - 600 V
175 - 600 V
Average value: 519 V Grade Count:22