Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.0 - 95.0 µm/m-°C @Temperature >=162 °C |
7.22 - 52.8 µin/in-°F @Temperature >=324 °F |
Average value: 54.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.22 µin/in-°F @Temperature 73.4 - 302 °F |
|
Budd DSM-971 Smooth Surface, Class "A" SMC
(discontinued **) Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer. |
|||
CTE, linear | 13.0 - 400 µm/m-°C | 7.22 - 222 µin/in-°F | Average value: 60.2 µm/m-°C Grade Count:46 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear | 13.0 µm/m-°C | 7.22 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
CTE, linear | 13.0 µm/m-°C | 7.22 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
CTE, linear | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP424 Laminate Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el.. |
|||
CTE, linear | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
CTE, linear | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP610 Paper Base Laminate Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne.. |
|||
CTE, linear | 13.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
7.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy® 183 Au-Ge Solder Alloy Eutectic die attach.Information provided by the manufacturer, Indium Corporation. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 - 100 °C |
7.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCONEL® Alloy 718 Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 - 100 °C |
7.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Goodfellow Gold 88/Germanium 12 Eutectic Alloy Special purpose solder.Information provided by Goodfellow. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 - 100 °C |
7.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 27.0 - 100 °C |
7.22 µin/in-°F @Temperature 80.6 - 212 °F |
|
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
AIM 88Au/12Ge Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
CTE, linear | 13.0 - 14.0 µm/m-°C | 7.22 - 7.78 µin/in-°F | x ,y direction; IPC TM-650 2.4.41 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
Armstrong C-7/W Epoxy Adhesive, 2:3 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
CTE, linear | 13.0 - 16.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
7.22 - 8.89 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 27.0 - 100 °C |
7.22 µin/in-°F @Temperature 80.6 - 212 °F |
|
Carlson C 201 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 23.0 - 100 °C |
7.22 µin/in-°F @Temperature 73.4 - 212 °F |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
CTE, linear | 13.0 - 55.0 µm/m-°C | 7.22 - 30.6 µin/in-°F | Average value: 26.6 µm/m-°C Grade Count:63 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
CTE, linear | 13.0 - 13.0 µm/m-°C @Temperature 180 - 180 °C |
7.22 - 7.22 µin/in-°F @Temperature 356 - 356 °F |
Average value: 27.9 µm/m-°C Grade Count:1 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
CTE, linear | 13.0 µm/m-°C @Temperature 20.0 °C |
7.22 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |