Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Budd DSM-971 Smooth Surface, Class "A" SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Polyester, TS
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Budd DSM-971 Smooth Surface, Class "A" SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
Water Absorption <= 0.35 %
<= 0.35 %
ASTM D570-63
Linear Mold Shrinkage 0.00070 cm/cm
0.00070 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Tensile Strength, Ultimate 70.0 MPa
10200 psi
ASTM D638-68
Flexural Yield Strength 175 MPa
25400 psi
ASTM D790-70
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790-70
Compressive Yield Strength 145 MPa
21000 psi
ASTM D695-69
Izod Impact, Notched 9.50 J/cm
17.8 ft-lb/in
ASTM D256-70
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 23.0 - 150 °C
7.22 µin/in-°F

@Temperature 73.4 - 302 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 235 °C
>= 455 °F
ASTM D648-61