Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy
Manufacturer Ceradyne Advanced Ceramics
Trade Name SEMICORE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft sealsLightweight generators, usually for aircraftVane actuators for missiles Particle beam focusing, quadrupoles, lenses, wigglers, etc.Magnetic bearings, gyros, vacuum pumps, accelerometers Various mechanisms in disk drives, cameras, tape drives, and miniature loudspeakers and earphones; where small size is important Magnetic alignment at 90° to compaction angle.Information provided by Ceradyne Company
Physical Properties Metric English Comments
Density 8.40 g/cc
0.303 lb/in³
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 10.5 W/m-K
72.5 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000500 ohm-cm
0.0000500 ohm-cm
Magnetic Coercive Force, Hc >= 1500 Oe
>= 1500 Oe
Intrinsic
8100 - 8500 Oe
8100 - 8500 Oe
Magnetic Remanence, Br 8500 - 9100 Gauss
8500 - 9100 Gauss
Magnetic Maximum Energy Product, BH 18 - 20 MGOe
18 - 20 MGOe
Curie Temperature 700 °C
1290 °F
Descriptive Properties Value Comments
Room Temperature Compensation, RTC, %/°C -0.045