Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.20 - 74.0 µm/m-°C | 4.00 - 41.1 µin/in-°F | Average value: 49.9 µm/m-°C Grade Count:28 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 7.20 - 113 µm/m-°C | 4.00 - 62.8 µin/in-°F | Average value: 55.8 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | at Set Pt. |
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 100 °C |
4.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott D 263® T eco Thin Borosilicate Optical Glass D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 - 300 °C |
4.00 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8806A Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 25.0 - 1000 °C |
4.00 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base Single component system with a paint consistency. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 952 High Temperature Ceramic Adhesive, Nickel Composition |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 1000 °C |
4.00 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL85C Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 1000 °C |
4.00 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL90N Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
|
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
|
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina Fine grain castable ceramic. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 7.20 - 150 µm/m-°C | 4.00 - 83.3 µin/in-°F | Average value: 48.9 µm/m-°C Grade Count:143 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear | 7.20 µm/m-°C @Temperature 20.0 °C |
4.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
CTE, linear | 7.20 µm/m-°C | 4.00 µin/in-°F | at Set Pt. |
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |