Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
modified; ASTM D696 |
Solvay Engineered Polymers DEXFLEX® 711-300 TPO
(discontinued **) Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color match.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG902L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG960 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMG302 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMG314V Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMG334V Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMH454 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® Rapide CLG 356B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® Rapide CLG 910B Enhanced Molding Acrylic Polymer Specially designed to reduce injection molding cycle times and therefore provide production cost benefits.Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1340 Crystal Polystyrene 1340 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades such as LACQRENE® 7240. In dilution, LACQRENE® 1340 gives excellent pro.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM D696 |
Total PSC 1450 High Heat Resistance, Easy Flow Crystal Polystyrene Total Petrochemicals Polystyrene 1450 is a high heat resistance, easy flow crystal polystyrene for injection molding and the foam extrusion industry. This product offers optimum fluidity and excell.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total PSC 1810/1811 Polystyrene 1811 is a very easy flowing crystal polystyrene designed, principally, for the injection molding industry. The excellent processing characteristics of this grade allows for the production of articl.. |
|||
CTE, linear | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
|
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |
Lucite International Diakon® CLG357 Acrylic Polymer Information provided by Lucite International |
|||
CTE, linear | 71.0 µm/m-°C | 39.4 µin/in-°F | ASTM E831 |