Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials N-Sil® RTV123 Silicone Modified Alkoxy Adhesive Sealants, Black N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
CTE, linear | <= 270 µm/m-°C @Temperature 20.0 °C |
<= 150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV6136 Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV615 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV6186 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV6196 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 400 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9070 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9275 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF3320 Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF4032 General Purpose Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF4451 High Surface Resistivity Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 700 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9030 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9050 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF4050 General Purpose Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF4420 High Heat Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
CTE, linear | 270 µm/m-°C @Temperature 20.0 °C |
150 µin/in-°F @Temperature 68.0 °F |
Silicone rubber component |
Saint-Gobain COHRlastic® CF4480 High Heat Reversion Resistant Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |