Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name COHRlastic®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durometer to the relatively hard 70 durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations. 9200 Series: COHRlastic 9200 High Performance Series provides excellent tensile strength and superior tear resistance. It is tougher and more resilient than general-purpose silicone. Standard thicknesses are 1/32", 1/16" and 1/8", and it withstands temperatures ranging from -100°F to +400°F. A minimum thickness of 0.015" is available on a minimum quantity basis. All data based on a 0.0625 inch test sample.(Also comes in thicknesses from 1/32" to 1/8") Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
Increases by 10 after dry heat aging for 70 hrs at 437°F.; ASTM D2240
Tensile Strength, Yield 8.27 MPa
1200 psi
Tensile strength decreases by 20% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Elongation at Break 600 %
600 %
Elongation properties decrease by 30% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Tear Strength 28.0 kN/m
160 pli
Initial Tear Strength; ASTM D624
Compression Set 30 %

@Temperature 160 °C
30 %

@Temperature 320 °F
Constant Deflection, 70 hrs.; ASTM D395
Thermal Properties Metric English Comments
CTE, linear 270 µm/m-°C

@Temperature 20.0 °C
150 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.26 J/g-°C
0.300 BTU/lb-°F
Thermal Conductivity 0.187 W/m-K
1.30 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
Descriptive Properties Value Comments
Color Gray