Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV6126 Clear Potting/Encapsulating Gel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depths. Typical uses: GP with very fast cure without heat and automated meter/mixing equipment.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Viscosity 750 cP

@Temperature 25.0 °C
750 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 270 µm/m-°C

@Temperature 20.0 °C
150 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Continuous useful temperature.
Optical Properties Metric English Comments
Refractive Index 1.41
1.41
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.8

@Frequency 1000 Hz
2.8

@Frequency 1000 Hz
Dielectric Strength 20.5 kV/mm

@Thickness 1.91 mm
521 kV/in

@Thickness 0.0750 in
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Cure time 5 min.
Pot Life 5.00 min

@Temperature 25.0 °C
5.00 min

@Temperature 77.0 °F