Polymer Property : CTE, linear = 14.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 25.2 µm/m-°C

@Temperature -40.0 - 149 °C
14.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet)
CTE, linear 25.2 µm/m-°C

@Temperature -20.0 - 150 °C
14.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E831
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
CTE, linear 25.2 - 190 µm/m-°C
14.0 - 106 µin/in-°F
Average value: 109 µm/m-°C Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
CTE, linear 25.2 - 27.0 µm/m-°C
14.0 - 15.0 µin/in-°F
Average value: 25.9 µm/m-°C Grade Count:5
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 25.2 µm/m-°C

@Temperature 22.8 - 260 °C
14.0 µin/in-°F

@Temperature 73.0 - 500 °F
ASTM E831
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide
Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Plaslube® J-50/20/SI/2 Polycarbonate, 20% GFR, 2% Silicone
CTE, linear 25.2 µm/m-°C

@Temperature -40.0 - 82.2 °C
14.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron EMERGEâ„¢ 8702 Polycarbonate
EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Tempalux® 20% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
CTE, linear 25.2 - 28.8 µm/m-°C

@Temperature 25.0 - 125 °C
14.0 - 16.0 µin/in-°F

@Temperature 77.0 - 257 °F
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material
PROTOBLOCK is a new composite material made of inorganic granules and epoxy resin engineered to form a micro-porous structure for use as prototype vacuum form or thermoform tooling. The material is..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 25.2 µm/m-°C
14.0 µin/in-°F
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
CTE, linear 25.2 µm/m-°C

@Temperature -40.0 - 149 °C
14.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T4301 Polyamide-imide, extruded bearing grade (ASTM Product Data Sheet)
CTE, linear 25.2 - 30.6 µm/m-°C
14.0 - 17.0 µin/in-°F
Average value: 28.2 µm/m-°C Grade Count:3
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear 25.2 µm/m-°C

@Temperature 20.0 °C
14.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 25.2 - 25.2 µm/m-°C

@Temperature 60.0 - 138 °C
14.0 - 14.0 µin/in-°F

@Temperature 140 - 280 °F
Average value: 25.2 µm/m-°C Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Copyright © lookpolymers.com All Rights Reserved