Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.8 - 38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 8.00 - 70.0 µm/m-°C | 4.44 - 38.9 µin/in-°F | Average value: 30.7 µm/m-°C Grade Count:10 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 65.0 - 70.0 µm/m-°C | 36.1 - 38.9 µin/in-°F | Average value: 69.5 µm/m-°C Grade Count:29 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear | 20.0 - 70.0 µm/m-°C | 11.1 - 38.9 µin/in-°F | Average value: 40.2 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.8 - 38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1000 PC (Asia Pacific) |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3025PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025PJ is a general use grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3027PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PJ is an extrusion grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3027PU(X) Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PU(X) is an extrusion grade.Information provided by Samyang. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3030PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3030PJ is a high viscosity gradeInformation provided by Samyang. |
|||
CTE, linear | 45.0 - 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 - 38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
CTE, linear | 45.0 - 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 - 38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON M-300P PCTFE Pellets NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries. |
|||
CTE, linear | 45.0 - 70.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 - 38.9 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON M-400H PCTFE Granular Molding Powder NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process.. |
|||
CTE, linear | 60.0 - 70.0 µm/m-°C | 33.3 - 38.9 µin/in-°F | |
Hippe PC Polycarbonate Hard, stiff, very good impact properties with a wide range of temperature (to -100°C). High stability of shape under heat. Clear with own slight yellowish color. Low water absorption, weather-re.. |
|||
CTE, linear | 60.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
CTE, linear | 65.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
36.1 - 38.9 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
CTE, linear | 65.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
36.1 - 38.9 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-9 Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C | 27.8 - 38.9 µin/in-°F | ASTM D696 |
Samyang Trirex® 3026B Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026B is an extrusion grade.Applications: BottlesInformation provided by Samyang. |
|||
CTE, linear | 26.0 - 70.0 µm/m-°C | 14.4 - 38.9 µin/in-°F | Average value: 39.7 µm/m-°C Grade Count:26 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |