Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 66.0 MPa
9570 psi
SABIC - Japan Method
Elongation at Break 220 %
220 %
SABIC - Japan Method
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 - 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
27.8 - 38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257