Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 60.0 - 100 µm/m-°C @Temperature 20.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
CTE, linear | 50.0 - 100 µm/m-°C @Temperature 20.0 °C |
27.8 - 55.6 µin/in-°F @Temperature 68.0 °F |
Cured |
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resist.. |
|||
CTE, linear | 23.0 - 100 µm/m-°C @Temperature >=162 °C |
12.8 - 55.6 µin/in-°F @Temperature >=324 °F |
Average value: 61.5 µm/m-°C Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
CTE, linear | 43.0 - 100 µm/m-°C | 23.9 - 55.6 µin/in-°F | Average value: 67.8 µm/m-°C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 60.0 - 100 µm/m-°C @Temperature 20.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 68.4 µm/m-°C Grade Count:25 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 58.6 µm/m-°C Grade Count:15 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
CTE, linear | 62.0 - 100 µm/m-°C | 34.4 - 55.6 µin/in-°F | Average value: 74.0 µm/m-°C Grade Count:33 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
CTE, linear | 42.0 - 100 µm/m-°C | 23.3 - 55.6 µin/in-°F | Average value: 59.5 µm/m-°C Grade Count:9 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 70.9 µm/m-°C Grade Count:42 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 63.3 µm/m-°C Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
CTE, linear | 65.0 - 100 µm/m-°C | 36.1 - 55.6 µin/in-°F | ASTM D696 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon FEP Fluorinated Ethylene Propylene Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t.. |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | ISO 11359 |
Styrolution Novodur® BX13036 ABS + PMMA Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution |
|||
CTE, linear | 80.0 - 100 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 - 55.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
CTE, linear | 95.0 - 100 µm/m-°C @Temperature 20.0 °C |
52.8 - 55.6 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 73.7 µm/m-°C Grade Count:34 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Average value: 85.0 µm/m-°C Grade Count:14 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Average value: 90.0 µm/m-°C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
CTE, linear | 100 - 100 µm/m-°C @Temperature -90.0 - -30.0 °C |
55.6 - 55.6 µin/in-°F @Temperature -130 - -22.0 °F |
Average value: 100 µm/m-°C Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
CTE, linear | 70.0 - 100 µm/m-°C | 38.9 - 55.6 µin/in-°F | Average value: 81.3 µm/m-°C Grade Count:16 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 79.7 µm/m-°C Grade Count:13 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 10.0 - 100 µm/m-°C @Temperature -100 - 250 °C |
5.56 - 55.6 µin/in-°F @Temperature -148 - 482 °F |
Average value: 21.2 µm/m-°C Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
CTE, linear | 7.00 - 100 µm/m-°C @Temperature 55.0 - 250 °C |
3.89 - 55.6 µin/in-°F @Temperature 131 - 482 °F |
Average value: 20.4 µm/m-°C Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
CTE, linear | 72.0 - 100 µm/m-°C | 40.0 - 55.6 µin/in-°F | Average value: 88.4 µm/m-°C Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |