CTE, linear 7.20 - 74.0 µm/m-°C
4.00 - 41.1 µin/in-°F
Average value: 49.9 µm/m-°C Grade Count:28
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
CTE, linear 7.20 - 113 µm/m-°C
4.00 - 62.8 µin/in-°F
Average value: 55.8 µm/m-°C Grade Count:4
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
at Set Pt.
Ferro EG 0026 Glaze and Sealant Glass
Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 - 100 °C
4.00 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet
Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Schott D 263 Thin Borosilicate Glass
D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Schott D 263® T eco Thin Borosilicate Optical Glass
D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 - 300 °C
4.00 µin/in-°F

@Temperature 68.0 - 572 °F
Schott S8806A Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
CTE, linear 7.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.00 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base
Single component system with a paint consistency.
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 952 High Temperature Ceramic Adhesive, Nickel Composition
CTE, linear 7.20 µm/m-°C

@Temperature 1000 °C
4.00 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL85C Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 7.20 µm/m-°C

@Temperature 1000 °C
4.00 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL90N Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
CMW® THERMKON® 70M Molybdenum Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina
Fine grain castable ceramic.
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
CTE, linear 7.20 - 150 µm/m-°C
4.00 - 83.3 µin/in-°F
Average value: 48.9 µm/m-°C Grade Count:143
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass
Data provided by the manufacturer, Owens Corning.
CTE, linear 7.20 µm/m-°C
4.00 µin/in-°F
at Set Pt.
Ferro EG 2964 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins..