Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CA - 41 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 71 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 82 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 82 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 51 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 87 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® MC5300 PC+ABS (Asia Pacific) Cycoloy MC5300 resin is a high heat, flame retardant PC/ABS blend. MC5300 resin passes UL-94 listing of 1.5mm V0 and 2.5mm 5VB. The balance of good flow, impact performance and heat resistance makes.. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific) |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 41 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 51 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 51 HF UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 81 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
CTE, linear | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D696 |
Kolon KOPA® KN333NW High Impact Nylon 66 Impact -resistant, dimensional safetyApplications Wheel coversInformation provided by API-Kolon. |
|||
CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 - 44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL TCN8222 PPE+HIPS (Asia Pacific) PPE/HIPS unfilled 80C FR-V2 |
|||
CTE, linear | 60.0 - 65.0 µm/m-°C | 33.3 - 36.1 µin/in-°F | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | Below Tg |
Tra-Con Tra-Bond F118 Fiber Optic Epoxy Adhesive TRA-BOND F118 is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows mor.. |
|||
CTE, linear | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2106 Fast Cure, Medium Viscosity Epoxy Adhesive TRA-BOND 2106 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This clear, two-part, medium viscosity syste.. |
|||
CTE, linear | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai.. |
|||
CTE, linear | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity.. |
|||
CTE, linear | 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
CTE, linear | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |