Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.8 µm/m-°C @Temperature -40.0 - 149 °C |
31.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature -40.0 - 149 °C |
31.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Quantum Polysulfone Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | NOVA Chemicals Laboratory Procedure |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
CTE, linear | 55.8 µm/m-°C @Temperature -40.0 - 149 °C |
31.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
CTE, linear | 55.8 µm/m-°C @Temperature -40.0 - 149 °C |
31.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
CTE, linear | 55.8 - 91.8 µm/m-°C | 31.0 - 51.0 µin/in-°F | Average value: 69.2 µm/m-°C Grade Count:9 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM E831 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-3810 TPO/TPE Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Westlake Plastics Radel® R Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Tempalux® Polyetherimide For Medical Applications Medical grade Tempalux is made from Ultem® polyetherimide resin, an amorphous thermoplastic which exhibits excellent resistance to a wide range of chemicals and disinfectants. Ultem maintains its .. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature 20.0 °C |
31.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications Medical grade Zelux GS polycarbonate is produced from resin formulated to meet the stringent performance characteristics and requirements of the healthcare industry. Suitable for EtO gas and limite.. |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |
|||
CTE, linear | 55.8 µm/m-°C @Temperature -40.0 - 149 °C |
31.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |