| Category | Polymer , Thermoplastic , Polyphenylsulfone (PPSU) |
| Manufacturer | Quantum Advanced Engineering Plastics |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quantum PPSU.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Water Absorption | 0.37 % | 0.37 % | ASTM D570 |
| Water Absorption at Saturation | 1.1 % | 1.1 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 80 | 80 | ASTM D785 |
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Hardness, Shore D | 80 | 80 | ASTM 2240 |
| Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Break | 60 - 120 % | 60 - 120 % | ASTM D638 |
| Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
| Flexural Strength | 91.0 MPa | 13200 psi | ASTM D790 |
| Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
| Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
| Shear Strength | 62.1 MPa | 9000 psi | ASTM D732 |
| Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
| Thermal Conductivity | 0.349 W/m-K | 2.42 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 218 °C | 424 °F | ASTM D3417 |
| Maximum Service Temperature, Air | 160 °C | 320 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 214 °C | 417 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 207 °C | 405 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz |
3.4 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D149 |
| Dissipation Factor | 0.00020 @Frequency 1.00e+6 Hz |
0.00020 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| FDA Compliance | yes |