Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Quadrant Engineering Plastics Products
Trade Name Quadrant PPSU
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.37 %
0.37 %
24 hour immersion; ASTM D570
1.1 %
1.1 %
saturation; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Hardness, Shore D 80
80
ASTM D2240
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Tensile Modulus 2.34 GPa
339 ksi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Compressive Yield Strength 92.4 MPa
13400 psi
10% deformation; ASTM D695
Compressive Modulus 1.93 GPa
280 ksi
ASTM D695
Shear Strength 62.1 MPa
9000 psi
ASTM D732
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
K (wear) Factor >= 2010 x 10<sup>-8</sup> mm³/N-M
>= 1000 x 10<sup>-10</sup> in³-min/ft-lb-hr
QTM 55010
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.349 W/m-K
2.42 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C
300 °F
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648
Glass Transition Temp, Tg 220 °C
428 °F
ASTM D3418
Flammability, UL94 V-0

@Thickness 3.10 mm
V-0

@Thickness 0.122 in
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Constant 3.44

@Frequency 1e+6 Hz
3.44

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.2 kV/mm
360 kV/in
ASTM D149
Dissipation Factor 0.0017

@Frequency 1e+6 Hz
0.0017

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA Yes
Yes
NSF No
No
USDA No
No
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Color black