Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.4 µm/m-°C @Temperature -20.0 - 150 °C |
8.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E831 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 14.4 - 21.6 µm/m-°C | 8.00 - 12.0 µin/in-°F | Average value: 18.9 µm/m-°C Grade Count:4 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
CTE, linear | 14.4 - 110 µm/m-°C | 8.00 - 61.1 µin/in-°F | Average value: 35.9 µm/m-°C Grade Count:53 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 14.4 - 16.2 µm/m-°C | 8.00 - 9.00 µin/in-°F | Average value: 15.5 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | |
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-1/CF/30/TF/15 Nylon 66, 30% Carbon Fiber Reinforced, PTFE Lubed Carbon Fiber Reinforced, PTFE Lubricated |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-1/CF/40 BK PA66 |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-1/CF/40 NAT PA66 |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 - 100 °C |
8.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCOLOY® Alloy 800 A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The.. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 - 100 °C |
8.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | ASTM-D696 |
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
CTE, linear | 14.4 µm/m-°C | 8.00 µin/in-°F | ASTM D696 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
CTE, linear | 14.4 - 16.2 µm/m-°C | 8.00 - 9.00 µin/in-°F | Average value: 14.8 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |