IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy

Category Metal , Nonferrous Metal , Beryllium Alloy , Nickel Alloy
Manufacturer IBC Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers these properties with the additional benefit of superior thermal conductivity. Beryllium nickel casting alloys are notable for their high resistance to wear, thermal shock, and corrosion even at elevated temperatures in the range of 1000°F (540°C).The 40 series BeNiCr Casting Alloys have historically been utilized for high definition precision cast jewelry and commemorative rings, as well as, dental component applications.Information provided by IBC Advanced Alloys.
Physical Properties Metric English Comments
Density 8.25 g/cc
0.298 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 95 - 100
95 - 100
Annealed
Hardness, Rockwell C 44 - 50
44 - 50
Annealed and Aged
Thermal Properties Metric English Comments
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
Melting Point 1150 - 1260 °C
2100 - 2300 °F
Solidus 1150 °C
2100 °F
Liquidus 1260 °C
2300 °F
Component Elements Properties Metric English Comments
Beryllium, Be 1.9 - 2.2 %
1.9 - 2.2 %
Chromium, Cr 0.45 - 0.80 %
0.45 - 0.80 %
Nickel, Ni 97 - 97.65 %
97 - 97.65 %
As Balance
Processing Properties Metric English Comments
Casting Temperature 1260 - 1370 °C
2300 - 2500 °F
Pouring Range