Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Carbon Fiber Filled |
Manufacturer | Techmer ES |
Trade Name | Electrafil® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Techmer ES Electrafil® J-1/CF/40 BK PA66.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Water Absorption | 0.60 % | 0.60 % | 24 Hrs; ASTM D570 |
Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 276 MPa | 40000 psi | ASTM D638 |
Elongation at Break | 1.8 % | 1.8 % | ASTM D638 |
Flexural Strength | 407 MPa | 59000 psi | ASTM D790 |
Flexural Modulus | 23.4 GPa | 3400 ksi | ASTM D790 |
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.4 µm/m-°C @Temperature 20.0 °C |
8.00 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 257 °C | 495 °F | ASTM D648 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |
Descriptive Properties | Value | Comments |
---|---|---|
Shielding @ 1 GHz | 30-40 db | ES7-83 |