Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | |
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 33% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | |
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced Vypet VNT 840 HY is a 40% glass/mineral reinforced PET high strength injection molding compound with improved hydrolysis stability designed for electrical and structural applications, with High Diel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-1/-2 |
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Polyram PlusTek RA325G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced, Flame Retardant, Halogen Free 30% Glass-fiber reinforced, flame retardant halogen free Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-93 |
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-93 |
Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | DIN EN ISO 75 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO R75 |
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | |
Arkema Group Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO R75 |
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | DAM; ASTM D648 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | As molded; ISO 75 A |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |