Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C @Thickness 3.18 mm |
430 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D-648 |
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM) Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Plenco 51130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF5 HS L 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compos.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF6 L BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEI/C GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF13 ML2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF13 SL2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Silicone LubricantFeatures: Lubricated and Heat StabilizedInformation pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66 LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Chem Polymer Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced A glass fiber reinforced, flame retardant nylon 6,6 exhibiting excellent tensile strength and high temperature performance. The material has VO flammability rating according to UL94 testing procedu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 |
Plenco 51030 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |