Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF5 L BK 5% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 1.8 %

@Time 86400 sec
1.8 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 86.2 MPa
12500 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.4 µm/m-°C
28.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 19.3 kV/mm
490 kV/in
Method A (Short-Time); ASTM D149