Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C @Thickness 6.35 mm |
421 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D-648 |
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ISO 75-1,-2 |
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ISO 75-1,-2 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ISO 75-1,-2 |
Gromax BFG50-BN00N1 Nylon 6 60% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C @Thickness 3.20 mm |
421 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Valox® 507 PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU), 30% Glass Fiber Veradel® AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Saint-Gobain Meldin® 3130 Thermoplastic Bearing Material Meldin 3130 components provide good strength and stiffness in addition to excellent high velocity performance. This formulation can be used with both hard or soft mating surfaces. Meldin® 3100 .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ISO 75-1, 2 |
Polyplastics Duranex® 7400F Polybutylene Terephthalate (PBT), Low friction, Low wear, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Adell AT-13 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Adell BR-37 Nylon 6, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Adell BR-38 Nylon 6, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Ashley Polymers Ashlene® 830LS-33G Nylon 6, 33% Glass Reinforced A 33% glass fiber reinforced and heat stabilized Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | Unannealed; ASTM D648 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C @Thickness 3.20 mm |
421 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 421 °F | ASTM D648 |
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |